Effects of geometric and material property changes on the apparent elastic properties of cancellous bone
(2009-04-24)
Osteoporosis is a disease characterized by reduced bone mass and reduced bone quality. This deterioration manifests itself in osteoporotic fractures at skeletal sites containing large proportions of cancellous bone (ie. ...